TECHNET Archives

June 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Marsico, James - ES" <[log in to unmask]>
Date:
Tue, 21 Jun 2011 14:15:43 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Bush, Jeffrey D. (US SSA)" <[log in to unmask]>
Message-ID:
Subject:
From:
"Bush, Jeffrey D. (US SSA)" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (64 lines)
I agree - TTM Santa Clara performs well with fused SnPb as well as selective plating with NI.

You may also want to push ENIG as the likely cause for the prohibition is the issues with embrittlement.  Discuss the IG process with your customer which will demonstrate gold levels far below the volumes needed to effect this condition.  I have found cold restrictions are not logically implemented in cases like this.

Jeffrey Bush
BAE Systems Incorporated 
IS&R - Space Products and Systems
P.O. Box 868, MER24-116A
Nashua, NH 03061-0868
Office +1 603.885.8137
Mobile +1 603.318.8056
Fax +1 603.885.5258


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Marsico, James - ES
Sent: Tuesday, June 21, 2011 2:00 PM
To: [log in to unmask]
Subject: [TN] HASL is becomming a Hassle...

Once again, we have a heritage space job that our customer prohibits HASL, because of the extra thermal excursion.  They also prohibit ENIG, reasons unknown.  We're having a hard time finding a PWB house that does plated and fused Sn60, space qualified.  Any recommendations?

Jim Marsico
ITT Corporation
1500 New Horizons Blvd.
North Amityville, NY 11701
631-630-5079
[log in to unmask]<mailto:[log in to unmask]>


________________________________
This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2