TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Busko, Wolfgang" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 15 Nov 2001 14:33:42 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (49 lines)
Hi Alejandro,
 
it may turn out that HASL is not the best choice for this application. With
this pitch and lower we love to have a more planar surface.
We had enough trouble with 0.8mm pitch and concave termination in the
beginning and a lot of pad-tuning had to be done. It turned out that the
manufacturer´s recommendations weren´t that bad at all (exept for the
excessive length of the pad, must have been for wavesoldering I guess).
Don´t think that a stepped stencil is necessary, it would make life more
complicated than necessary. Better control the amount of paste with the
aperture size.
 
Would be nice to have a test board with different layouts for that purpose,
wouldn´t it?
 
Good luck 
 
Wolfgang

-----Ursprüngliche Nachricht-----
Von: Becerra Alejandro [mailto:[log in to unmask]]
Gesendet am: Mittwoch, 14. November 2001 15:42
An: [log in to unmask]
Betreff: [TN] Resistor Networks of 0.5 mm Pitch


Hello to All, 
we are planning to start using resistor networks of 0.5 mm pitch 
in a normal reflow soldering process. The boards are FR-4 with HASL coating.

Is there any special concern about this component? 
So far the smallest resistor network that we are using is a 0.8 mm pitch. 
Within my company it is being recommended a stepped stencil for this
component. Is this necessary? 

Thanks, 

Alejandro Becerra 

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2