Hi Alejandro,
it may turn out that HASL is not the best choice for this application. With
this pitch and lower we love to have a more planar surface.
We had enough trouble with 0.8mm pitch and concave termination in the
beginning and a lot of pad-tuning had to be done. It turned out that the
manufacturer´s recommendations weren´t that bad at all (exept for the
excessive length of the pad, must have been for wavesoldering I guess).
Don´t think that a stepped stencil is necessary, it would make life more
complicated than necessary. Better control the amount of paste with the
aperture size.
Would be nice to have a test board with different layouts for that purpose,
wouldn´t it?
Good luck
Wolfgang
-----Ursprüngliche Nachricht-----
Von: Becerra Alejandro [mailto:[log in to unmask]]
Gesendet am: Mittwoch, 14. November 2001 15:42
An: [log in to unmask]
Betreff: [TN] Resistor Networks of 0.5 mm Pitch
Hello to All,
we are planning to start using resistor networks of 0.5 mm pitch
in a normal reflow soldering process. The boards are FR-4 with HASL coating.
Is there any special concern about this component?
So far the smallest resistor network that we are using is a 0.8 mm pitch.
Within my company it is being recommended a stepped stencil for this
component. Is this necessary?
Thanks,
Alejandro Becerra
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|