TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 19 May 2009 15:02:10 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Werner Engelmaier /* <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (409 lines)
 Bev,
I am afraid you may not get anything better than what I said already.
Werner


 


 

-----Original Message-----
From: Bev Christian <[log in to unmask]>
To: [log in to unmask]; [log in to unmask]
Sent: Tue, 19 May 2009 2:38 pm
Subject: RE: [TN] Underfill Pass/fail criteria

























Werner,



Yes, this is a very nice article. I remember
reading it now.  This gives some guidelines for characteristics of the material. 
However, what I am looking for are visual/instrumental measurement parameters
for saying whether the cured underfill under a CSP or BGA is good or not.



Bev



RIM
















From:
[log in to unmask] [mailto:[log in to unmask]] 

Sent: Tuesday, May 19, 2009 2:18
PM

To: [log in to unmask]; Bev Christian

Subject: Re: [TN] Underfill
Pass/fail criteria






 






Hi Bev,

Clearly, the most important SJs that need to be covered are the outermost rows
and the rows directly underneath the die outline—this later is most important
for face-up BGAs and CSPs.

I do not know if one can write generally applicable pass/fail criteria
[because, what else, 'It depends'].

I ave attached a column of mine on underfills [sorry for the rest of you for
whom IPC strips the attachment], Engelmaier, W., “Reliability Improvement with
Underfill,” Global SMT & Packaging, Vol. 6, No. 3, March 2006, pp. 66-67. 

Werner









 









 






----
-Original
Message-----

From: Bev Christian <[log in to unmask]>

To: [log in to unmask]

Sent: Tue, 19 May 2009 1:51 pm

Subject: [TN] Underfill Pass/fail criteria




TechNetters,





I am aware of J-STd-030 "Guideline for Selection & Application of





Underfill" and the existence of IPC standards committee 5-24F "Underfill





Adhesives for Flip Chip Applications".  There is nothing in IPC-A-610D





about underfills.  I have taken Brian Toleno's very good course on





underfills, but on going back and looking at the CD, I don't see





anything on pass/fail criteria.  Do any of you know of an international





standard (American, IEC, Japanese) with pass/fail criteria for cured





underfills?











I am particularly interested in what said standard (or anything you want





to tell me) says about coverage and voiding.











Bev





RIM











---------------------------------------------------------------------





This transmission (including any attachments) may contain confidential 





information, privileged material (including material protected by the 





solicitor-client or other applicable privileges), or constitute non-public 





information. Any use of this information by anyone other than the intended 





recipient is prohibited. If you have received this transmission in error, please 





immediately reply to the sender and delete this information from
 your system. 





Use, dissemination, distribution, or reproduction of this transmission by 





unintended recipients is not authorized and may be unlawful.











---------------------------------------------------





Technet Mail List provided as a service by IPC using LISTSERV 15.0





To unsubscribe, send a message to [log in to unmask] with following text in





the BODY (NOT the subject field): SIGNOFF Technet





To temporarily halt or (re-start) delivery of Technet send e-mail to 





[log in to unmask]: SET Technet NOMAIL or (MAIL)





To receive ONE mailing per day of all the posts: send e-mail to 





[log in to unmask]: SET Technet Digest





Search the archives of previous posts at: http://listserv.ipc.org/archives





Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 





additional information, or contact Keach Sasamori at [log in to unmask] or 





847-615-7100 ext.2815





-----------------------------------------------------











--------------------------------------------------------------------- 

This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this inf
ormation from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2