Great info! What is the 1.5 million cycles equate to in usage time.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gerard O'Brien
Sent: Monday, April 25, 2005 7:14 AM
To: [log in to unmask]
Subject: Re: [TN] ENIG vs Hard Gold
Alistair - as part of the 4552 specification testing, we ran ENIG at 2
microinches for 1.5 million cycles for a keypad type application. We
stopped
because the membrane was breaking down but not the ENIG surface. The
data
can be found in the tech paper that is in the appendix of IPC-4552
Regards
Gerard O'Brien
Photocircuits Corporation
Co-chairman 4-14
-----Original Message-----
From: Alistair Murray [mailto:[log in to unmask]]
Sent: Monday, April 25, 2005 6:51 AM
To: [log in to unmask]
Subject: [TN] ENIG vs Hard Gold
Hi to everyone,
Could someone please let me know or indicate where I can obtain
information on the relative performances of ENIG and Hard Gold in
keyboard applications?
Many thanks in anticipation.
Alistair Murray
Artetch Circuits Ltd
UK
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|