TECHNET Archives

June 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Whittaker, Dewey (AZ75)" <[log in to unmask]>
Date:
Thu, 3 Jun 2004 06:35:46 -0700
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Bergman <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Whittaker, Dewey (AZ75)" <[log in to unmask]>
Parts/Attachments:
text/plain (99 lines)
David,
You are right and we are taking that position also. The problem is that my
customers are requiring me to report the use of(amounts and percentages, per
site and part number)any of the materials identified in the WEEE or RoHS
documents. Besides being a cost and time burden, there is a fear when the
first person's knee buckles, we will all have to things that have no merit,
such as being halogen-free.
Dewey

-----Original Message-----
From: David Bergman [mailto:[log in to unmask]]
Sent: Wednesday, June 02, 2004 2:32 PM
To: [log in to unmask]
Subject: Re: [TN] How about Halogen free FR4?


Hi Eddie,

You are mistaken regarding the European directives.  There are no
directives that require FR-4 to be bromine free.  This is a very common
error.  The primary flame retardant in FR-4 is TBBPA and this is not
regulated by the RoHS directive.

So if you are looking to change, your drivers for change should be other
than legislative ones.

Best regards,
Dave



David W. Bergman, CAE
Vice President Standards, Technology and International Relations,
IPC
2215 Sanders Road #250
Northbrook, IL 60062-6135
Dir. Line 847-790-5340  Main 847-509-9700
Mobile 847-867-1388
Dir. Fax 847- 504-2340   Main Fax 847-509-9798
E-mail [log in to unmask]    web www.ipc.org



-----Original Message-----
From: Eddie Rocha [mailto:[log in to unmask]]
Sent: Wednesday, June 02, 2004 3:58 PM
To: [log in to unmask]
Subject: [TN] How about Halogen free FR4?

I've asked two top laminate mfg'rs on their status with halogen free
FR4 and both only manufacture this in Europe. I believe the
European directives require FR4 to be halogen / bromine free. Am I
mistaken or should we all be concerned with laminate also?

-- Thanks,
Eddie Rocha
(408) 978-8992 x 282

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2