TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Larry Russell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 22 Nov 2004 14:47:55 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (104 lines)
Our testing for RoHS states
"Collection of test data pursuant to Section 25 of the German Foodstuffs and Commodities Act..."

I prefer my biscuits salted, lead optional. Precious metals are attractive as packaging, though.
Did someone mistake the use of these biscuits and chocolate boards and require them to be food grade?


Larry Russell 

-----Original Message-----
From: Reuven ROKAH [mailto:[log in to unmask]]
Sent: Sunday, November 21, 2004 3:24 PM
Subject: Re: English expression


We call it "Chocolate board".


Best  Regards

Reuven  ROKAH

e mail: [log in to unmask]



                      Guenter
                      Grossmann                To:      [log in to unmask]
                      <Guenter.Grossma         cc:
                      [log in to unmask]>              Subject: [TN] English expression
                      Sent by: TechNet
                      <[log in to unmask]
                      >


                      18/11/2004 18:19
                      Please respond
                      to TechNet
                      E-Mail Forum;
                      Please respond
                      to Guenter
                      Grossmann





Hi all
When small PCBs are assembled and soldered they are together in a
larger unit and separated after the production.
Whats the English expression of this unit. In German we call that
"Nutzen" (that's for Werner it might help him to understand what I
mean).

Thanks a lot for your help

Guenter

EMPA
Swiss Federal Laboratories  for Materials Testing and Research
Centre for Reliability
Guenter Grossmann,  Senior Engineer

8600 Duebendorf
Switzerland

Phone: xx41 1 823 4279
Fax :     xx41 1 823 4054
mail:     [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2