TECHNET Archives

May 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
peter blokhuis <[log in to unmask]>
Date:
Fri, 18 May 2001 13:00:30 -0100
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Ken Mc Gowan <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Ken Mc Gowan <[log in to unmask]>
Parts/Attachments:
text/plain (60 lines)
Hi Peter,

US normally specifies Co whereas Europe is predominantly Ni. Electrically
there are no major differences. Co deposits can be up to 20% harder under
certain conditions. I agree about dragout/dragin this is usually controlled
by the use of Au strike.

Best Regards,

Ken Mc Gowan
----- Original Message -----
From: "peter blokhuis" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, May 16, 2001 6:17 PM
Subject: [TN] Cobalt or Nickel hardened gold?


> Does anyone know why Cobalt much more prevalent than
> Nickel as a hardener in electrolytic gold plating?
>
> From the plater's perspective, nickel seems to make
> more sense since this is dragged into the gold tank
> from the nickel plating tank upstream.  This dragover
> serves as an automatic hardener addition, thus
> simplifying process control.
>
> Do any of you assemblers out there specify Cobalt? Why?
>
> __________________________________________________
> Do You Yahoo!?
> Yahoo! Auctions - buy the things you want at great prices
> http://auctions.yahoo.com/
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2