Can anyone out there recommend a good masking tape?
Desired properties, in approximate order of importance:
1. Withstands 85C indefinitely.
2. Sticks well, but peels off without leaving residue.
3. Antistatic a plus, but conductive probably not worth it (we
use ionizing air blowers).
4. Inexpensive.
Our coatings are mostly urethanes, manually sprayed.
Joe Kane
BAE SYSTEMS Controls
Johnson City, NY
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|