Technet,

We use an X-ray flourescence scope to measure solder
thickness and composition. Recently, we sent samples
to a university to have the composition measured by
Edacs (I probably spelled that wrong). In case I 
spelled that wrong and you don't know what I mean -
Edacs composition measurements are a by-product of
scanning electron microscopes. Anyway, the tin-lead
percentages we got from Edacs were way different from
the results we got on our X-ray. I'm thinking this
might be because the Edacs measures an extremely small
surface area whereas the X-ray measures a 5 to 10 mil
diameter circle.

Does anyone have any experience with SEM and/or Edacs
in relation to solder composition? We would appreciate
any info to confirm my theory or refute.

Thanks,
Dave Hall
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2