TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 28 Sep 2006 12:20:52 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Phil Nutting <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
Has anybody defined recommended maximum copper thickness (weight) with
specific size SMT components?
 
For example; 2 oz. copper max with 0603 resistors and caps.
 
My thoughts process here is I know that with thicker copper there is
more undercut by the etchant.  There must be a point of diminishing
returns for pad size to maintain good manufacturing capabilities, not to
mention the remote possibility of rework.
 
Some of our "power electronics" boards may be specified as 4 oz. copper
for the large power components, but this might be an issue for the small
control circuit components like 0603 foot prints.
 
Thanks in advance.
 
Phil Nutting

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2