TECHNET Archives

September 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Tue, 21 Sep 2010 10:36:21 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (155 lines)
The IAg will be completely dissolved into the solder, leaving you to form your IMC with the brass. How well does that work?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Thayer, Wayne - IIW
Sent: Tuesday, September 21, 2010 10:22 AM
To: [log in to unmask]
Subject: Re: [TN] Solderability of nickel plating

Why nickel? I use ImAg over brass for lots of stuff around here.  Works great, but will tarnish over time.

Wayne

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Tuesday, September 21, 2010 9:38 AM
To: [log in to unmask]
Subject: Re: [TN] Solderability of nickel plating

OK, pardon the lack of knowledge, but why is that?  I also see reference to nickel-boron platings, which supposedly improve both conductivity and solderability for electronics applications.

Is it recommended then that I need to apply gold over the EN on this electrical tab?  A portion of it is soldered (internally) and a portion of it remains exposed for connection (think 120V plug tabs).  The base material is brass.

Kevin Glidden
Manufacturing Engineer
Astronics Luminescent Systems Inc.

-----Original Message-----
From: vladimir Igoshev [mailto:[log in to unmask]]
Sent: Tuesday, September 21, 2010 9:24 AM
To: TechNet E-Mail Forum; Glidden, Kevin
Subject: Re: [TN] Solderability of nickel plating

Kevin,

You wouldn't want to solder directly to unprotected  E-Ni.
Vladimir

SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca

-----Original Message-----
From: "Glidden, Kevin" <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date:         Tue, 21 Sep 2010 08:52:39
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
        "Glidden, Kevin" <[log in to unmask]>
Subject: [TN] Solderability of nickel plating

All,

Can anyone comment on the solderability of the nickel plate, particularly with regard to type of plating: high phosphor / low phosphor, and also storage conditions:

I've been gathering info, and seen conflicting information.

From one article: http://corrosion-doctors.org/MetalCoatings/Electroless.htm

A paper submitted at the Electroless Nickel conference of 1989 held in Cincinnati Ohio, Titled "Solderability Parameters of Elecroless Nickel Bearing Electronic Finishes" By Louis Kosarek of STB Systems, Inc. report that "An electroless nickel deposit which contains a concentration of phosphorus ranging from 0.1% to 3.0% is readily solderable on an "As-plated Basis" per Mil-Std 883c method 2003. The frequency of solderability tests which fail per Mil-Std 883c will increase as the phosphorus content of electroless nickel alloy increases from 3.0 to 7.0% phosphorus. A solderability test conducted per Mil-Std 883c method 2003 incorporating an as-plated surface finish containing phosphorus in excess of 7%, the components will consistently fail. The mode of failure is non-wetting of the surface."
This indicates low phosphorous plating is best for solderability.  Many other papers seem to agree with this.

---------------------------------------------------------------------------------------------------------------------

From another article: http://www.pfonline.com/articles/pfd0024.html

Solderability/Weldability.  An important aspect of electroless nickel to the electronics industry is its solderability. All electroless nickel deposits are solderable provided the soldering conditions are matched to the condition of the particular electroless nickel deposit. Lower-phosphorus electroless nickel is more easily solderable immediately after plating than higher-phosphorus electroless nickel. However, this advantage disappears after 12 - 24 hrs. At this point, the ease of solderability depends upon the characteristics of the passive layer that forms on the surface of the electroless nickel deposit. Those deposits plated from baths containing heavy metal and sulfur-bearing brighteners and stabilizers, such as most commercial low- and mid-phosphorus electroless nickel systems, form a thicker tenacious passive layer than those that do not, such as most high-phosphorus electroless nickel systems. High-phosphorus electroless nickel systems tend to be more solderable in aged deposits.

Other important factors influencing the solderability of electroless nickel deposits include residual contamination left on the surface after plating and storage conditions after drying. Surface contamination and exposure to environments containing sulfur dioxide, chlorine, high humidity and high ambient temperatures will detrimentally affect solderability. Therefore, it is imperative that parts be thoroughly rinsed in clean DI water, dried and stored in a cool, dry atmosphere, preferably nitrogen.
This article indicates high phosphorous plating is best for long term solderability, and also that parts must be stored carefully (cool, dry, sealed, nitrogen).  Other articles seem to state this is a highly stable finish and is even used as a corrosion inhibitor.

Thanks,


Kevin Glidden
Manufacturing Engineer
Astronics Luminescent Systems Inc.<http://www.astronics.com>
4 Lucent Drive
Lebanon, NH 03766
(603) 643-7766 x3152

Please note, LSI operates on a 9/80 work schedule, and is closed on alternating Fridays.  Please click the link provided to view the days LSI will be closed.
http://www.astronics.com/LSI/documents/2010calendar-NH.pdf

NOTICE: This communication is intended specifically for the recipient(s) named above and may include proprietary, confidential or privileged information. If you are not a named recipient, you should immediately delete or destroy all electronic and physical copies of this communication. Unintended recipients also should not utilize, repeat, publish or relay to any other person the information contained herein nor should they take any action based upon, in whole or in part, such information. If you have received this message in error, you are requested to contact the sender immediately.

EXPORT COMPLIANCE STATEMENT: The information contained herein is or may be controlled by the International Traffic in Arms Regulations (ITAR), 22 CFR 120-130, or the Export Administration Regulations (EAR) and may not be exported, or disclosed to a foreign person, whether in the United States or abroad, without prior U.S. Government and Astronics Luminescent Systems written approval. Violations of these regulations could result in administrative, civil or criminal penalties.  If you have any questions about the nature of the material contained in this email please contact the sender immediately.


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2