Though I have not seen the solderballs prior to
assembly, they do have an impact. Generally, they move around the board
during reflow and stick where you want them the least. I.e. gold plated
contacts, etc. Depending on the pitch of the parts used for assembly,
you may also see shorts.
Simply cleaning the boards prior to assembly usage takes
care of them and their associated problems.
Cobey Schmidt
VisionTek
-----Original Message-----
From: Erat, Wolfgang
[SMTP:[log in to unmask]]
Sent: Friday, June 05, 1998 8:56 AM
To: [log in to unmask]
Subject: [TN] SOLDERBALLS on
bareboards
Hello Techs
Is there a criteria for solderballs at the
bareboard level ? prior to
assembly ?
Have you seen solderballs from the HASL process
? Would this affect the
assembly process or would any solderballs simply
reflow ?
Thanks in advance for your input /
Wolfgang Erat / QA Manager / Viasystems Canada
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service
by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to
[log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full
name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site
(http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at
[log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|