TECHNET Archives

March 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Nieznanski, John A - Exelis" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Nieznanski, John A - Exelis
Date:
Tue, 3 Mar 2015 15:36:43 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (28 lines)
Good Morning TechNet!

Has anyone experienced or documented any examples (photos, DPA reports, chemical analysis, etc.) of the type of dielectric staining referenced in the Rogers application note below? This concern applies to composite PTFE laminates with a large volume fraction (>50%) of ceramic filler particles.

http://www.rogerscorp.com/documents/643/acm/The-Prevention-and-Removal-of-Absorbed-Chemicals-in-Ceramic-Filled-PTFE-Composites.pdf

Key Excerpts:

The material's high filler loading also contributes to approximately 5 volume percent porosity.
Low surface tension liquids such as organic solvents and surfactant laden aqueous solutions can penetrate the pores.
Failure to adequately rinse these laminates following exposure to process chemicals can sometimes result
in dielectric staining or increased dielectric loss.

I think we may be dealing with this issue and would appreciate any relevant details you may wish to share (specific dielectric materials, photos, DPA reports, chemical analyses, dispositions/resolutions, etc.)

Thank you!

John Nieznanski

________________________________

This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of Exelis Inc. The recipient should check this e-mail and any attachments for the presence of viruses. Exelis Inc. accepts no liability for any damage caused by any virus transmitted by this e-mail.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2