Howard,
Would you provide me with more information like:
1. How long you have been using Thermabond?
2. What is the life expectancy of the application (i.e., will the
Thermabond still be adhering the heatsink to the pwb near end-of-life?)?
3. What environmental conditions (temp & humidity extremes) will the
Thermabond be exposed to?
Any info in this area would be quite helpful.
Thanks,
Mike Adams
Lucas Aerospace
[log in to unmask]
(216)995-1195 x3058
> ----------
> From: Howard Feldmesser[SMTP:[log in to unmask]]
> Sent: Thursday, October 16, 1997 4:24 PM
> To: [log in to unmask]
> Subject: Re: [TECHNET] Heatsink lamination
>
> Marty,
> We've had very bad luck with bonding heatsinks with prepreg,
> most
> often resulting in a board that looks like a potato chip. Several
> years
> ago we switched to Arlon's Thermabond with great success. We've
> launched
> several satellites with bonded on heatsinks and all are still
> functional, a
> true test of surviving rigorous use.
> Howard Feldmesser
> The Johns Hopkins University Applied Physics Laboratory
>
> At 2:54 PM 10/16/97 -0400, Sheppard, Marty - LYPME wrote:
> >We are attempting to attach a nickel-plated copper heatsink to a 10
> >layer PWB per a set of manufacturing drawings that only states that
> "the
> >heatsink shall be attached with prepreg". It does not call out a
> >pressure, temperature, cycle time, or a type of prepreg. We have
> >assumed that we would need a "low-flow" type of prepreg. We have
> tried
> >some sample cards with a low-flow prepreg (PC-GF 108V by Westinghouse
> >Fortin) that we have on hand; we have had good registration of the
> >heatsink to card, but the adhesion has not been as good as we would
> have
> >liked, and the heatsink seems to have been pressed "into" the board
> (you
> >can feel the outline of the heatsink on the backside of the card).
> We
> >ran the press at the lowest possible pressure we can for our press
> (15
> >lbs).
> >
> >We are looking for suggestions from anyone who has experience with
> >laminating heatsinks to PWBs.
> >
> >Thanks,
> >
> >Marty W. Sheppard / LYPME
> >Manufacturing Engineering Support
> >(912)-926-9632 DSN 468-9632 Fax: (912)926-7974
> >email: [log in to unmask]
> >
> >##############################################################
> >TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> >##############################################################
> >To subscribe/unsubscribe, send a message to [log in to unmask] with
> following
> >text in the body:
> >To subscribe: SUBSCRIBE TECHNET <your full name>
> >To unsubscribe: SIGNOFF TECHNET
> >##############################################################
> >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> >information.
> >For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> >847-509-9700 ext.311
> >##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|