Water is the most classic of all solvents, Bill, and probably dissolves
more substances than any one organic solvent :-)

Brian

[log in to unmask] wrote:

> Need to be precise when you ask a question like this- do you mean a 'cleaning
> agent' (which covers all the families) or are you limiting it to the solvent
> family? Classic solvents are those which would be used in defluxing/degreasing
> equipment, or are volatile enough to be used for manual (post-touchup)
> cleaning. (see IPC SC-60A).
> Suggest you review the Aqueous (IPC AC-62A) Cleaning Handbook & the
> Semi-Aqueous (IPC SA-61A) Cleaning Handbook for information on the other cleaning agent
> families.
> [The Kyzen materials Doug cites can be found listed under Type II in the
> SA-61A.]
>
> Bill Kenyon
> Global Centre Consulting
> 3336 Birmingham Drive
> Fort Collins, CO   80526
> Tel: 970.207.9586   New Cell: 970.980.6373
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2