Phil: The ingredient common to most anti-stat formulations is virtually the same sort of ingredient in hair conditioners... (think that a hair conditioner really is noticeable because the hair does not build up a charge) and also fabric softeners. The ingredient is a surfactant (detergent) with a positive charge.
My suspicion is that the better they work, the shorter the time they will work. In other words, the more effective a particular surfactant is at dissapating charge, the more readily it is removed.
This is strictly FYI..
Rudy Sedlak
RD Chemical Company
Phil Nutting <[log in to unmask]> wrote: Has anybody used any of the available anti static sprays to reduce
"static ticking" in a high voltage environment?
On doing a web search I see there are many products on the market, but
are these really for ESD control?. The question is, do I have to keep
re-spraying the item to keep it functioning or is it a one time
application?
Thanks in advance.
Phil Nutting
Design for Manufacturing Engineer
Kaiser Systems, Inc.
126 Sohier Road
Beverly, MA 01915
voice: 978-922-9300 x1310
fax: 978-922-8374
e-mail: [log in to unmask]
www.kaisersystems.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Yahoo! Music Unlimited - Access over 1 million songs. Try it free.
|
|
|