TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"(George Milad)" <[log in to unmask]>
Date:
Wed, 15 Jul 1998 20:54:27 EDT
Content-transfer-encoding:
7bit
Content-type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (27 lines)
Gold wire bonding: requires adequate thickness of a compatible metal, these
may be gold or palladium. Examples are:
Electrolytic Ni with Electrolytic soft gold (>20 uins)
Electroless Ni with Electroless gold (>20 uins)
Electroless NI with electroless Pd (10-15 uins) with immersion gold flash (1
uins)
Traditionally immersion gold at < 5 uins  has limited success for gold wire
bonding.
Electroless Ni (150 uins) with Immersion gold (>5uins) is  an ideal finish for
Al wire bonding.  The Al wire bonds readily to the underlying Ni.

George Milad
Technical Mkt Mngr
LeaRonal Inc

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2