TECHNET Archives

March 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Blomberg, Rainer (FL51)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 1 Mar 2000 08:48:08 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (64 lines)
Marvin,

A simple test for cleanliness is what we call the "water break free" test.
Apply D.I. water to the surface to be tested and observe how well the water
wets the surface.  It should flow out, onto the surface and not bead up
(like on a waxed surface).  As the water flows off the surface, when the
sample is held vertical, it should sheet off in a thin film and not bead on
the surface for 5-10 seconds.  Another method is to apply a few drops to the
horizontally held surface and judge the angle the meniscus makes.  The
cleaner the surface, the shallower the angle.  As for identifying the
contamination, we typically use SEM and IR Spectroscopy.
Hope this helps.

-----Rainer Blomberg

-----Original Message-----
From: marvin v. picardal [mailto:[log in to unmask]]
Sent: Wednesday, March 01, 2000 6:34 AM
To: [log in to unmask]
Subject: [TN] How to detect contamination on metal surface


Dear Techneters,

I would like to ask some information as to
how to detect contamination on metal surface and
how do I determine what type of contamination that is.
The said contamination results to poor adhesion
between the glue and the metal surface.

I do hope you would take time in helping me out with this.
Thank you in advance.

Marvin

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2