TECHNET Archives

May 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 28 May 2003 14:15:41 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bill Decray <[log in to unmask]>
Subject:
From:
Bill Decray <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (94 lines)
I agree it look like a open to me as well. Since it is at a angle it will be
very difficult to place a weld there. As far as the finish copper half oz
foil should have been used unless a waiver from the customer was provided to
use 1 oz. I would also ask for a cross section of the board as well. How did
the open pass electrical test?
Just my thoughts.


Highest Regards,

William W. DeCray III
PHONE:(434) 237-6391 ext 115
CELL:   (434) 851-6115
FAX:    (434) 237-1324


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Steve
Gregory
Sent: Wednesday, May 28, 2003 1:53 PM
To: [log in to unmask]
Subject: [TN] Trace thickness problem...


Hi all!

I'd like your opinion on something. We're building a prototype assembly for
a
customer, and discovered something at final inspection that we didn't see
when we received the bare fabs. We ordered 16-boards in four, 4-up panels.

We found a trace that has a spot where it looks like it didn't plate up
during final plating. Take a look at "Trace Thickness" at
http://www.stevezeva.homestead.com

There's 4-boards we've found that have this problem, 1 on one panel, and 3
on
another panel, and of course they're all built up. The 6012 says that
thickness can't be reduced by more than 20% of the minimum conductor
thickness. I
can't really tell if it's 20% or 50%.

I've sent pictures both to our customer and the fab vendor. The customer
wants the spot repaired, and there are a number of ways to do that. The fab
vendor
says it's not a problem because the stack-up drawing calls out 1-oz. copper
after plating on the surface layer, and they said that there's more like
2-oz.
on the surface layer, so there shouldn't be any problem, at least that's
what
I was told, I didn't speak to anyone directly. The stack-up is on my page
too,
look at "Stack-up"...

The first question that comes to my mind, if 1-oz after plating was called
on
the stack-up, why was 2-oz plated? Or is that normal?. The drawing
references
our customers internal spec for fabrication, but it uses MIL-PRF-55110 for
references.

What are your opinions about this?

Thanks everyone!

-Steve Gregory-



---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2