Gerald G. Gagnon wrote:
> Hello All
>
> I am in need of density values for:
>
> Electrolytic "hard" gold used for card edge fingers
> Electrolytic "soft" gold used for wire bonding
> Immersion gold used for solderable surface
>
> The above would reflect the deposit metallurgy typically expected for
> each end use.
>
> Thanks and regards
>
> Gerry
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
Gerry,
I amalso interested.Please resend any information to me too.I think that
I could use it in my XRF
appliccations.But, what do you think about the problem of different
suppliers with different bath
formulations and processes?
Bye,
Gaby
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|