TECHNET Archives

September 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 25 Sep 2017 07:55:55 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Peter Barton <[log in to unmask]>
Message-ID:
Subject:
From:
Peter Barton <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Laser?



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of TechNet automatic digest system

Sent: 23 September 2017 06:00

To: [log in to unmask]

Subject: TechNet Digest - 18 Sep 2017 to 22 Sep 2017 (#2017-153)



There is 1 message totaling 42 lines in this issue.



Topics of the day:



  1. Thin alumina substrate cutter



----------------------------------------------------------------------



Date:    Fri, 22 Sep 2017 18:09:21 +0000

From:    Ioan Tempea <[log in to unmask]>

Subject: Thin alumina substrate cutter



Dear Technos,



I need to cut some narrow strips out of 0.005" thick microstrip alumina substrates. The diamond tips we have do an acceptable job on the substrate, but tend to lift the corners of the 50 ohms trace.



Is there any special tool for this kind of surgery?



Thanks,



Ioan Tempea, P. Eng.

Senior Manufacturing Engineer, Satellite Systems



[cid:[log in to unmask]]



MacDonald, Dettwiler and Associates Corporation, 21025 Trans-Canada Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2

Tel: +1-514-457-2150 x3556

www.mdacorporation.com<https://urldefense.proofpoint.com/v2/url?u=http-3A__www.mdacorporation.com_&d=DwIFaQ&c=3eL_sJZ3ltkdBrwH9pzZyHVgRtGZOGAKdghkf0hTlAQ&r=x7LMoVvKp_RWxHd2sGo83xt7HEWakRyuwQbmfz0jKVcba101DaldZ00b6KCmUS-M&m=nUqsmFNvFwQ3ftxHQyP3NouGT4RU55DwIZhlnei-HGI&s=sb3t4XArtR6o0YRjWVrfUGH06ArNXjqAnamnU8f8eX4&e= >



This e-mail, and any attachments, are intended solely for the use of the intended recipient(s) and may contain legally privileged, proprietary and/or confidential information. Any use, disclosure, dissemination, distribution or copying of this e-mail and any attachments for any purposes that have not been specifically authorized by the sender is strictly prohibited. If you are not the intended recipient, please immediately notify the sender by reply e-mail and permanently delete all copies and attachments. This email is for informational purposes only and shall not be interpreted to authorize or conclude a binding agreement between MDA and any other party unless this email contains or is accompanied by an express written confirmation of MDA's intention to enter into a binding agreement, such confirmation shall only be provided by an authorized representative of MDA.



------------------------------



End of TechNet Digest - 18 Sep 2017 to 22 Sep 2017 (#2017-153)

**************************************************************


ATOM RSS1 RSS2