TECHNET Archives

February 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Michael McMonagle <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Michael McMonagle <[log in to unmask]>
Date:
Wed, 15 Feb 2006 09:12:51 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (66 lines)
Fredrik,
        You can order standardizing solution and other supplies/parts for
your Omega Meter from www.scscoatings.com, the division of Cookson that now
handles the ionic test equipment....

Mike McMonagle
Quality Manager
OYO Geospace
7007 Pinemont Drive
Houston, TX 77040
Ph 713-986-8650
Fx 713-986-8725

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Skillborg, Fredrik
Sent: Wednesday, February 15, 2006 8:28 AM
To: [log in to unmask]
Subject: [TN] Resistivity calculator

Hello,



I am trying to bring life to an old Omega Meter but cannot get hold of
fresh Standardizing solution #3. Is there any calculator/table that
allows me to use some other concentration of the standardizing solution?

The nomgram from the manual only have a "calibration point" for the #3
solution.

Maybe this is a question that should have been put 25 years ago when the
equipment was new...



Thanks in advance.

// Fredrik




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2