The scientists an engineers that develop the press fit connectors must
have some kind of recommendation for press-fit connector applications.
What does AMP recommend for their product applications?


Wally Doeling (wallyd) wrote:
>
>         On the other hand, we have been using press-fit into Immersion
> gold/Electroless Nickel, with press-fit connectors for 3 years with no
> problems.
>         The press-fit connectors are Nickel/Gold plated and the gold on
> gold provides the lubricant.
>         Most gold plated press-fit connector pins are underplated with
> nickel also.
>         The trick is to control the hole size to give a good press fit,
> without distorting the fiberglass
> in back of the hole.
>         It does work!  And works well.
>         [log in to unmask]
>
>         -----Original Message-----
>         From:   Paul Gould [SMTP:[log in to unmask]]
>         Sent:   Monday, October 06, 1997 10:16 AM
>         To:     [log in to unmask]
>         Subject:        Re: [TECHNET] Press Fit and Ni/Au Surface Finish
>
>         Gus Morvillo wrote:-
>         >I am looking into E Ni/ I Au surface finishes, and have heard
> of a concern
>         >about press fit connectors and barrel cracking. Has anyone
> experienced this
>         >problem?
>         >Would there be a retention force issue, with one removal and
> re-insert?
>         Hi Gus,
>
>         E Ni/I Au is not recommended for press fit for two reasons.
>         Firstly, solder acts as a lubricant to pin insertion and forms a
> gas
>         tight seal which is why it is recommended for press fit.
>         Secondly, Electroless Nickel is brittle and fractures which
> could result
>         in stray metal causing subsequent connector shorts. Also, there
> is no
>         gas tight seal formed which could lead to future corrosion.
>
>         We produce many multi-layer backplane pcb's for global companies
> and
>         they still specify tin-lead, either Reflowed or HASL. I have not
> seen
>         any other alternatives mentioned or been asked to come up with
> one.
>
>         Best Regards
>         Paul Gould
>         [log in to unmask]
>         Teknacron Circuits Ltd
>         Isle of Wight,UK
>
>         ##############################################################
>         TechNet Mail List provided as a free service by IPC using
> LISTSERV 1.8c
>         ##############################################################
>         To subscribe/unsubscribe, send a message to [log in to unmask]
> with following text in the body:
>         To subscribe:   SUBSCRIBE TECHNET <your full name>
>         To unsubscribe:   SIGNOFF TECHNET
>         ##############################################################
>         Please visit IPC web site (http://www.ipc.org/html/forum.htm)
> for additional information.
>         For the technical support contact Dmitriy Sklyar at
> [log in to unmask] or 847-509-9700 ext.311
>         ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################