We just got a lab report back saying we fail REACH because of an excess of cobalt.  The lab is trying to tell us it's the cobalt in the copper on the PCB and ICs.

I tend to believe something else was ground up with the board, accidentally or purposefully.  They did include the piezo sounder hanging off the board.