Hi Chris,
While I don't have any experience with Titanium, we do use it on PCB gold
fingers mostly to repair them for solder splashes. Strip as much solder
from the fingers as possible, plate nickel down, then gold over top. It
does work very well.
Steve
On Wed, Feb 23, 2022 at 6:26 AM Chris Knudsen <[log in to unmask]> wrote:
> Victor: sorry to interject, but,
>
> Steve,
>
> That product looks intriguing. Would you be willing to share your, or
> your company's, experience in using it?
>
> Can one reliably use several plating layers from a base material (say
> perhaps Titanium) to transition to a final gold plating, over a surface
> area of about 1.75 in^2 (11.3 cm^2)?
>
>
> -Chris
>
> Chris Knudsen, Principal Engineer • *New England Research, Inc.* • 331
> Olcott Dr Ste L1 • WRJ, VT 05001 • USA
> [log in to unmask] •
> https://linkprotect.cudasvc.com/url?a=https%3a%2f%2fwww.ner.com&c=E,1,0qUm5k__PccoHf_X8LuNoBCWlbzwBCpFN91bMZ0e8V1_uw_MwnWaHXEMgWciBSY1GbAFWwIkalyYkWJFWap2fm78VZPwTkxW4c-jZwWu8Xs2rhi5TZdASGyUuw,,&typo=1
> • Phone: +1-802-296-2401
>
>
> On Tue, Feb 22, 2022, at 9:37 AM, Steve Gregory wrote:
> >
> https://linkprotect.cudasvc.com/url?a=https%3a%2f%2fwww.hunterproducts.com%2fstore-pen%2f&c=E,1,aVZvQS3SLjp7OJS62mORQFHgPbPDq-_lulbYlDhJ_uxezZyPgucL5c7eGonBEpK0NBtSNqb5Nvvxy-pk-Pf277g6gljD3FXOtaTZ74mcJic1-wmH9yE,&typo=1
> >
--
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133
Cell Phone: (918) 706-2779
--
This email and any attachments are only
for use by the intended
recipient(s) and may contain legally privileged,
confidential, proprietary
or otherwise private information. Any
unauthorized use, reproduction,
dissemination, distribution or other
disclosure of the contents of this
e-mail or its attachments is strictly
prohibited. If you have received
this email in error, please notify the
sender immediately and delete the
original.
|