TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Thu, 31 May 2007 06:57:51 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (89 lines)
Good Morning Terry!

Although I don't have any experience with this material, it looks very,
very interesting. Check this out:

http://www.stablcor.com/presentation/ 

At the last company I worked at we were about to try the material in a
single board computer assembly that we had the task of ruggedizing, but
we ran into some issues with our customer that I won't get into...

Only drawback that I can initially see is that it is electrically
conductive and only licensed to a half-dozen fabs shops here in the US.
Maybe there might be some way that you can use this in your design.

Steve Gregory

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Terry Kozlyk
Sent: Thursday, May 31, 2007 6:02 AM
To: [log in to unmask]
Subject: [TN] Conductive Cooling thru Pre-Prig material

Technetters;

 

I have a 6 layer PCB with about 8 HOT DPAK components. The tabs are
electrically hot so I cannot just draw the heat directly thru a copper
fill brought out to the edge of the PCB.

 

I need electrical isolation, BUT high thermal conductivity between 2
adjacent layers.

 

Can anyone recommend what material they have specified to be used for
pre-prig that conducted the heat to the adjacent layer?

 

Voltage max is about 50 volts so I could probably go down to 2 or 3 mil
pre-prig.

 

Nothing special about this PCB; about 5" x 5".

 

The fab houses I solicited for info still haven't replied so I am
curious.

 

Any leads, products or websites would be appreciated.

 

Regards

TDK


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2