Set up a process using Dupont Vertrel SMT and Axerel 32 as a co-solvent in a
dip, vapor, distillate rinse. The process is still in use (for reasons that
are beyond me).
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Steve Gregory
Sent: Monday, August 21, 2006 8:52 AM
To: [log in to unmask]
Subject: [TN] Vapor Degreaser...
Good Mornining All!
Just curious, are there any of you out there still using a vapor
degreaser? If so, what are you using in it?
We have a Baron Blakeslee MLR-120 that looks in pretty good shape and
we're thinking about using it for certain
cleaning applications. I've been looking at some Enviro Tech
Ensolv-Ionic solvent to use in it.
There's been some suggestions to use alcohol in it, but I don't think
that's a very good idea considering the flammability
of alcohol. But besides that, alcohol isn't a very good solvent anyway.
Just wondering if anybody is still vapor degreasing anymore...
Thanks!
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|