TECHNET Archives

April 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Ivan Barrios <[log in to unmask]>
Date:
Mon, 24 Apr 2000 15:52:06 -0600
Content-type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (25 lines)
Hello Technetters:
We are trying to go to No clean flux in our wave solder process. However,
we still run some of these products with water soluble paste in SMT. We
will still wash the boards after SMT to remove any of the residues from SMT
process. Any issues foreseen with mixing the two types of manufacturing
practices (No clean and Water soluble) in the same product? (corrosion,
reactivation of crystalized WS flux while it passes thru wave, etc)
Any and all responses are welcome

Ivan Barrios

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2