Arnaud,
Not cheap, but FTIR is an excellent method for detecting silicones.
Regards,
Bev
-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of GRIVON Arnaud
Sent: Tuesday, January 7, 2020 9:00 AM
To: [log in to unmask]
Subject: [TN] [COM] Evaluating/Monitoring Silicone Contamination
Happy New Year TechNet !
Here is a first query for 2020...
We all know about the need of carefully segregate acrylic/urethane from
silicone conformal coatings, but how about evidencing and demonstrating (say
for an angry auditor) the actual lack of silicone cross-contamination on
toolings, ovens and workspaces ?
Are you aware of any reliable test system to perform silicone contamination
evaluations? What are their principles and related test methods & acceptance
criteria?
It looks like some suppliers offer Surface Silicone Contamination Test Kits
:
- Henniker
Plasma<https://plasmatreatment.co.uk/wp-content/uploads/2016/09/Henniker-Pla
sma-Technology-Overview.pdf> :
https://plasmatreatment.co.uk/henniker-plasma-technology/products/surface-te
st-equipment/test-for-surface-silicone-contamination/
- Anderson Materials Evaluation :
http://www.andersonmaterials.com/test_methods/testing-facilities-for-silicon
e-contamination.html#<http://www.andersonmaterials.com/test_methods/testing-
facilities-for-silicone-contamination.html>
Any practice of such test kits and return of experience to share?
Thanks in advance for your feedbacks.
Best regards,
Arnaud Grivon