Try this method using a scrap board first to get a feeling of the fine details. Mask board area around the connector with hi temp tape or other material. Preheat board in an oven. Place board on a solder wave fixture. Have one person slide the fixture over the wave till connector is right over the solder and another pull up gently and easy the connector after about 8 seconds.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Poh Kong Hui
Sent: Friday, November 05, 2004 8:57 AM
To: [log in to unmask]
Subject: Re: [TN] Removal of Connector
Hi Technetters,
I am facing an issue with a board of 10 layers and 2mm thick, gold plated.
I need to remove a 72 pin through hole connector. However, I am not able to
remove the connector using solder iron & solder sucker.
I understand if I am to use solder pot, I should be able to remove it. But
I do not have a mini-solder pot.
I am wandered if there is other way to take out the connector. Can someone
help to advise me other methods to remove the connector.
Thanks.
Poh
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|