Barbara,
Well, you have heard IAG, OSP, HASL
All are good if you can use them.
For us, the only finish that could replace Pb HASL was IAg.
OSP, ISn and Pb-free HAL have issues that stop their value in the designs we do.
I have to agree with George that IAg is probably best.
I'm open to off-line discussion if you want.
FNK
Frank N Kimmey CID+
Manager - PCB Design
Powerwave Technologies Inc
Mobile - 916-670-0645
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Barbara Burcham
Sent: Wednesday, June 01, 2011 6:17 PM
To: [log in to unmask]
Subject: [TN] Best Board Finish - beyond gold
Hey Y'all,
I am looking for a reliable bare board finish that beats the cost of gold.
What experience is out there?
What would you recommend?
Thanks,
Barbara Burcham
pcb Trace Design
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Click the following link to report this email as spam: https://www.mailcontrol.com/sr/DgYi3fKtTgnTndxI!oX7Us7Qlo!t9IHtALqD66c5HFYwqf9TVMlfscEFpzOrBxhv9YCwgKCA4hoLtzovJ!KJwA==
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|