Steve replied already but you didn't say if you wanted water soluble or solvent soluble. For water soluble I actually used peppermint lifesavers one time. Had run out of the standoffs. The location of the part precluded using a removable standoff. I bet I get some responses to this one.
-----Original Message-----
From: Ted Edwards [mailto:[log in to unmask]]
Sent: Friday, December 20, 2002 8:54 PM
To: [log in to unmask]
Subject: [TN] Disolveable Standoffs
I seem to remember that there at standoffs to set the height of a component off the PWB in assembly; but not who makes the ones that can be dissolved so they do not remain with the assembly. Anybody know who makes them?
Ted Edwards
Dynaco Corp.
--------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------