TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Scott Decker <[log in to unmask]>
Date:
Fri, 21 Apr 2006 16:35:08 -0400
Reply-To:
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (66 lines)
Diamond shape because when the solder wets out to the corners of the land
the pattern is not simply a squashed ball, but has for distinct gray
corners. I first heard this DFM guidance from Glenbrook. But, I have also
heard it argued that these land patterns may produce stress points that
could lead to reduced service life in of the joint. I don't have data to
support the argument against the square or diamond land pattern design. They
are not commonly used.
I will say this, a key hole pattern, that can be produced by a non-solder
mask defined land, can give a similar result. A distinct gray pattern where
the solder wets down the trace leaving the pad.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Scott Decker
Sent: Friday, April 21, 2006 1:40 PM
To: [log in to unmask]
Subject: [TN] BGA and CGA pad questions.


All,
   I was talking with our Manufacturing engineer the other day and the
people that make the SMD re-work station tools, about the pads used for
both BGA's and CGA's. The vendor was saying that diamond pads, (square
on a 45') were better for X-Ray inspection because you can see the pad
verses the pin/ball better during the inspection of the solder joints.
The X-Ray manufacturer' says the same thing, but has anyone done it this
way yet? It sounds good to me, but does anyone have any practical
experience with the diamond pads? How do you figure size between round
to square, etc.? Is it just area calculations or flat side the same as
diameter, etc.? Paste Mask sizing, Solder Mask defined, (not my thought)
or just the standard oversize, etc.? These would be for high-reliability
applications and from what I understand, the CGA is better in that
respect. Any info would be great to hear. Thanks in advance.


Scott Decker
AKA: Padmasterson
Broad Reach Engineering CAE
Ph. 480-377-0400 Ext. 34
FAX. 480-968-4597
Tempe, AZ.


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2