TECHNET Archives

April 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Torres, Roberto" <[log in to unmask]>
Date:
Fri, 26 Apr 2002 12:57:43 +0300
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Brian Ellis <[log in to unmask]>
Parts/Attachments:
text/plain (92 lines)
Bob

There are at least ten softwares available which allow you to crop what
you don't wish to see (and otherwise enhance the image). I use Corel
PhotoPaint, part of the Corel Draw! Suite, but there are more expensive
ones, such as PhotoShop which will do exactly the same job. I think
Ulead make a good one, as well and you may even find freebies or
shareware on the 'Net. Cropping and resampling also allow you to reduce
the file size if you wish to send images by e-mail, without any further
compression or other loss of image quality.

Best regards,

Brian

"Torres, Roberto" wrote:
>
> Brian;
>
> Well noted, just looks odd on the .jpg files.
>
> Bob
> -----Original Message-----
> From: Brian Ellis [mailto:[log in to unmask]]
> Sent: Wednesday, April 24, 2002 11:12 PM
> To: TechNet E-Mail Forum.; Torres, Roberto
> Subject: Re: [TN] Microscopes
>
> Roberto
>
> Does this matter? If you use a 4.3 or higher Mpixel camera, there are
> sufficient pixels left in the centre zone to record what you need to
> see, nicht war?
>
> Brian
>
> "Torres, Roberto" wrote:
> >
> > All;
> >
> > Thanks for the suggestions on Microscopes and Digital photographs.
> > The suggestion from Charles was of particular interest. Seems like
> > most use the method we use here now put the digital camera to the
> > lens of the microscope and snap away, it is just with this method
> > we tend to get a lot of telescope images, that is round and black
> > around the edges.
> >
> > Again thanks for all the input.
> >
> > Regards
> > Bob Torres
> >
> >
> ----------------------------------------------------------------------------
> -----
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> > To unsubscribe, send a message to [log in to unmask] with following text in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
> SET Technet NOMAIL
> > To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at: http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> >
> ----------------------------------------------------------------------------
> -----
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2