TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vS2jN-0000UOC; Mon, 25 Nov 96 09:13 CST
Encoding:
56 Text
Old-Return-Path:
Date:
Mon, 25 Nov 96 09:11:37 cst
Precedence:
list
Resent-From:
From [log in to unmask] Tue Dec 3 09:
49:17 1996
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/7982
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"ECLdj1.0.AkE.pURco"@ipc>
Subject:
From:
"ddhillma" <[log in to unmask]>
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
Cc:
Message-Id:
Parts/Attachments:
text/plain (66 lines)
     Good Morning!
     
     Question: What kind (alloy and temper designation) of metal were the 
     retaining pins made from? What is the maximum temperature of the 
     molding process and what do the pins see? You may have changed the 
     retention pin material properties during the molding operation.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: "Drape" of Material
Author:  [log in to unmask] at ccmgw1
Date:    11/25/96 8:40 AM


     
     Greetings,
     I have an acquaintance in the industry with an interesting problem.
     
     He is molding a flex circuit (2mil polyimide/one mil Cu)into a 
     particular circular shape. The circuit has PTH's at each end which 
     slip over pins for retention of the circuit during the molding 
     process. The circuit is on the outside of the bend.
     
     The first one hundred prototypes molded  without incident.
     
     The next lot of six hundred do not posses the same physical 
     properties. They will not conform to the shape of the tool. 
     When forced into this shape, as before, they no longer stay 
     in place. The retention pins that functioned flawlessly before, 
     during the one hundred piece run, now will not retain the circuit.
     
     I'm assuming that they were produced at the same facility, both times, 
     but have no evidence to support this.
     
     What happened?
     
     Thanks in advance.
     
     The views stated here are not necessarily those of my employer.
     
     
     [log in to unmask]@internet
     602.276.7361
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2