TECHNET Archives

December 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Franklin D Asbell <[log in to unmask]>
Date:
Wed, 27 Dec 2000 10:47:57 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, sean clinton <[log in to unmask]>
Subject:
From:
sean clinton <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
Organization:
Sanmina Plant 3
MIME-Version:
1.0
Parts/Attachments:
text/plain (58 lines)
Franklin,

One test I perform as a spot check to evaluate debris under the resist is to
look at a core after resist exposure for dents/debris/scratches...etc...I
mark the cover mylar by circling any suspect spots with a good ol Sharpee
marker and then run the core through my developer.  I then overlay the mylar
sheet keeping orientation the same as the original, and then observing the
circled areas.

This simple non empirical test gave us insight into how our material was
being handled.  It seems our lifting when we had it came from slight dents
and creased cores that could not conform to the resist allowing for resist
lifting.

Typically we use RTF foil, and a chemical clean process (no microetch)  Talk
to Rudy Sedlak of RD Chemical about it.  We get great adhesion with minimal
loss of copper (read as no increase in overall surface topography) and still
obtain excellent conformation on 1.5 and 1.2 mil resists.  I hope this helps
you out.

The only problem with my test is that it requires a person to visually
inspect a core for debris and dents on an imaged layer...Tough to do even if
you are good at it.  Happy hunting.


Sean Clinton
Sanmina Plant 3
Santa Clara, CA

Franklin D Asbell wrote:

> Yes, been spending much time in there...The lifting is isolated to very
> small areas (in comparison to the panel size) around .050".
>
> Of course it is identified under trace's after developing (AOI) and etch
> (AOI and visual inspection).
>
> My thoughts are it is also debris trapped under the resist and not a
> contaminate of the copper itself, if this makes sense.
>
> Any advice from all of you on DOE's performed in this area would be
> helpful, I'm developing one at the moment but want to make sure I
> include appropriate variables.
>
> Thanks,
>
> Franklin

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2