TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, pras chop <[log in to unmask]>
Date:
Fri, 10 Mar 2006 06:56:48 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Amol (349)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Kane, Amol (349)" <[log in to unmask]>
Parts/Attachments:
text/plain (54 lines)
Leaded or Lead-free Solder?

Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing 
941 Route 38  Owego, NY 13827
Phone: (607) 687-7669 x349
[log in to unmask]

 -----Original Message-----
From:   TechNet [mailto:[log in to unmask]]  On Behalf Of pras chop
Sent:   Friday, March 10, 2006 6:33 AM
To:     [log in to unmask]
Subject:        [TN] 0306 package

Hi,

  We are using an 0306 package for one of our boards. And we have been observing a lot of de-wetting,tombstone and no solder at times.

  Have anybody used these packages and experienced any such issues. Can anyone give details about the stencil aperture opening and other process requirement for this.

  Any ideas for using this package and to solve the above issues??

  Thanks in advance.

  Rgds
  Prashant


---------------------------------
 Jiyo cricket on Yahoo! India cricket

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Yahoo! Messenger Mobile Stay in touch with your buddies all the time.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2