TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
>From willli Thu Jul 17 08:
29:53 1997
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Thu, 17 Jul 1997 09:40:43 -0400
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/14077
From [log in to unmask] Mon Jul 21 11:
51:55 1997
X-Sender:
TO:
Return-Path:
<TechNet-request>
X-Loop:
Mime-Version:
1.0
Resent-Message-ID:
<"dRBdS.0.sOK.0vXpp"@ipc>
Subject:
From:
Denis Meloche <[log in to unmask]>
Cc:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0woqcj-000BjhC; Thu, 17 Jul 97 08:29 CDT
X-Mailer:
Windows Eudora Pro Version 3.0 (32)
Message-Id:
Parts/Attachments:
text/plain (50 lines)
In a previous life as a thick film engineer I purchased die from 

Elmo Semiconductor
N Glen Oaks Blvd
Burbank, CA 91504 USA 
818-768-7400 

Ask for electrical reject die for wirebonding.  If you ask for just reject
die you may get them missing bond pads.  

Denis Meloche
Heraeus Cermalloy
610-825-6050

At 04:30 PM 7/17/97 +0800, you wrote:
>
>Hi
>
>Does anyone know where I can purchase some dummy dies (say 200 pcs)  for
>wirebonding purposes?
>Thanks.
>
>Regards
>Richard
>
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
>* with <subject: subscribe/unsubscribe> and no text in the body.          *
>***************************************************************************
>* If you are having a problem with the IPC TechNet forum please contact   *
>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
>***************************************************************************
>
>
>

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2