TECHNET Archives

December 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Paul Wilson <[log in to unmask]>
Date:
Tue, 1 Dec 1998 06:32:13 -0500
X-To:
"Tumibay, Aleli" <[log in to unmask]>
Organization:
Circuit Center Inc.
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Paul Wilson <[log in to unmask]>
Parts/Attachments:
text/plain (76 lines)
Lei Tumibay,

The representation of units in terms of micrograms NaCl / sq cm is by convention only.
If one is interested in the sum of results of these ions expressed in these units, then

ppm F X (59/19) X 1000 = fluoride expressed as micrograms NaCl / sq cm
ppm Br X (59/80) X 1000 = fluoride expressed as micrograms NaCl / sq cm
ppm Cl X (59/36) X 1000 = fluoride expressed as micrograms NaCl / sq cm
ppm I X (59/127) X 1000 = fluoride expressed as micrograms NaCl / sq cm
ppm SO4 X (59/96) X 1000 = fluoride expressed as micrograms NaCl / sq cm

ppm etc X (59 / gram equivalent weight of etc) X1000 = etc expressed as micrograms NaCl / sq cm

The SUM of the results = all anions expressed as micrograms NaCl / sq cm

                        Paul Wilson
        R&D Manager / Plant Chemist

                   Circuit Center, Inc.
                 4738 Gateway Circle
                  Dayton, OH 45440

          Phone (937) 435-2131     Fax (937) 435-7698
            http://www.circuitcenter.com


-----Original Message-----
From:   Tumibay, Aleli [SMTP:[log in to unmask]]
Sent:   Monday, November 30, 1998 10:43 PM
To:     [log in to unmask]
Subject:        [TN] Q on Ion Chromatography

For the IC experts out there, I have questions for you:
        Our specs specify that "Package contamination" values be expressed in
ug NaCl equivalent / sq cm.   However,  the Ion Chromatography results that we
obtained are specific, itemized (i.e. Fl, Br, I, Cl, SO4, etc) and in ppm.
        1. What "anions" in the IC results are considered "NaCl equivalent"? (Do
I add all of the anions or is it just the Cl- ions?)
        2. If the total surface area of the unit and the IC solvent volume were
known, I can readily convert the IC results (ppm or mg/L) to ug/cm sq.  Am I
doing it right?  Or are these units not related to each other and therefore not
convertible?
Would appreciate all your responses.

Thanks,

Lei Tumibay
Lead Finish Group - Assembly Engineering
Analog Devices - General Trias
Cavite, Philippines
E-mail: [log in to unmask]
http://www.analog.com

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2