TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dave Seymour <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Dave Seymour <[log in to unmask]>
Date:
Fri, 15 Sep 2006 14:26:01 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (78 lines)
Here is an ESD link with technical support and some downloads.

http://www.charleswater.co.uk/tech.asp

dave


Dave Dixon wrote:

>Bob,
>        I haven't referenced them for quite some time, but the EOS/ESD
>Association (esda dot org) used to have a lot of available, and
>helpful publications.  I'm not sure of the difference between the
>pricing for non-members vs. members, but it may be a place to start.
>Best of luck,
>Dave
>
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Wilson
>Sent: Friday, September 15, 2006 12:06 PM
>To: [log in to unmask]
>Subject: ESD protection
>
>Hey everyone,
>
>Happy Friday!
>
>Can anyone point me to the best way to set up a shop floor for ESD
>protection?
>
>Thanks a bunch.
>
>Regards,
>
>Bob Wilson
>Electro-Mechanical Designer, CID
>SpectraSensors, Inc.
>972 N. Amelia Ave.
>San Dimas, CA 91773
>800-619-2861 x239
>www.spectrasensors.com
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>

--
Dave Seymour, CID+
Catapult Communications Inc.
800 Perimeter Park Dr, Suite A
Morrisville, NC 27560

Direct: (919)653-4249
Main: (919)653-4180
Fax: (919)653-4297

[log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2