Was there a Type O in the IPC-TM-65 stated reference #. Is it TM65 or TM650? What is the latest Rev.?
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Tuesday, May 29, 2012 9:26 AM
To: [log in to unmask]
Subject: Re: [TN] Spot test for Rosin Residue
Many thanks Brian!!
Rich Kraszewski
PLEXUS
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Thursday, May 24, 2012 1:35 AM
To: [log in to unmask]
Subject: Re: [TN] Spot test for Rosin Residue
Later: I was fairly sure I had it so did a deeper search and found it
in chapter 24.2 on p.279, pretty much as I described. I also bring to
your attention chap. 24.3 on the same page, the IPC acetonitrile test
which can also be used to detect the presence of rosin. The ref in the
book was
IPC-TM-65. Test Methods 2.3.38 and 2.3.39, Surface Organic Contaminant
Detection and Identification Tests, The Institute for Interconnecting
and Packaging Electronic Circuits, Evanston, II (1984).
obviously updated since then!
Brian
On 24/05/2012 03:18, Bev Christian wrote:
> Rich,
> Check this out.
> http://cool.conservation-us.org/coolaic/sg/bpg/pcc/10_spot-tests.pdf
>
>
> Section 10, Page 24 Spot Tests. The reference at this point is Barrow 1969,
> 13, TAPPI T408. I did not follow this up.
>
> I have never used the test myself.
>
> Bev
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
> Sent: Wednesday, May 23, 2012 6:28 PM
> To: [log in to unmask]
> Subject: [TN] Spot test for Rosin Residue
>
> I seem to recall a wet chemical spot test for rosin residues.
>
> Something that required:
>
> * Piece of filter paper.
> * Sugar solution .
> * Dilute Sulfuric acid.
>
> If the final spot went red, it would indicate the presence of rosin.
>
> Does anybody recall this test and have the details?
>
> Thanks in advance
>
> Rich� Kraszewski
> Plexus Engineering Solutions
> �
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|