Doug,
Is there any chance the mold could be made out of aluminum? There would be
no issue with solvents to remove the epoxy if an aluminum mold was used.
All of our molds are aluminum except for prototype molds which are made from
a Dow Corning Sylastic product.
Phil Nutting
-----Original Message-----
From: Douglas Pauls [mailto:[log in to unmask]]
Sent: Wednesday, March 21, 2001 11:27 AM
To: [log in to unmask]
Subject: [TN] Epoxy and Polycarbonate
Good morning all,
I have a polycarbonate fixture here used for potting connectors with a two
part epoxy material. After some use, the epoxy needs to be cleaned out of
the fixture holes. Right now, a drill is used, but does nasty things on
the hole tolerances. Do any of you chemically minded people know of a
solvent which will dissolve an epoxy coating, but which will not harm a
polycarbonate?
Doug Pauls
Rockwell Collins
SillyCorn Valley
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|