TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 21 Nov 2001 18:31:52 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (99 lines)
Hi, John,

Welcome to TN. I have to answer your question with more questions, like:

1) Are the problem components used anywhere else on the board and are they
  being properly wetted in those other positions?
2) What board finish are you using?
3) What is the termination finish of the components? Do they have any
  silver content for any reason?
4) How old are the components and what conditions have they been stored
  under?
5) Are the same locations failing to wet each time, or are some wetting in
  some cases and others in others?
6) What solder are you using?

I suspect you have an oxidisation problem with the component leads, perhaps
leeching of silver if there is any silver content. If it's a silver
problem, try using a 2% silver solder to redress the balance. If it's
oxide, you will have to replace the components or re-tin them in a solder
pot with a very aggressive flux.

Maybe I can help more with more detail.

Peter Duncan





                    John Brown
                    <johnbrown118@HO        To:     [log in to unmask]
                    TMAIL.COM>              cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST
                    Sent by: TechNet        Aero/ST Group)
                    <[log in to unmask]        Subject:     [TN] Non-wetting
                    >


                    11/21/01 04:54
                    PM
                    Please respond
                    to "TechNet
                    E-Mail Forum."






Good Morning, this is my first posting to this forum I hope to get some
help. We are building a small PWB with 4 per panel. The problems we are
encountering are on 0603 resistors & capacitors and SOIC (8pin) etc. These
are all located near to or the center of the PWB. There is paste on the pad
and the component placed properly but the paste will not wet onto the leads
or terminations.
What have we done?
1. Run the PWB at various profiles even the highest. Still have problem.
2. Changed from no clean to aqueous with an agressive flux. Still have
problem.
3. Changed screen apertures. Still have problem.
This PWB is multi layer and heavily populated.
Are there any hints as to what we do next?

_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------





[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2