Yep, effectively solder flows towards heat. 
At least it melts first in the hottest area and then, now being mobile,
surface tension/wetting forces will tend to pull it there. The flux, which
is temperature activated, will also be most effective initially in the first
heated areas.
Eventually heated area becomes uniform, all the solder will melt, and then
things may even up [as much as the geometry of wettable area and remaining
flux effectiveness allows].


Regards
 
Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Monday, June 28, 2010 7:11 PM
To: [log in to unmask]
Subject: Re: [TN] QFP short at top of the leads

Hi,

 That dull gray makes me thing of reflow without any flux. Was that SAC
paste with PbSn on the parts? If so maybe the PbSn reflowed first and for
some reason was pulled to the body. (Does solder really flow towards the
heat?)

Bob Kondner

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jerry Dengler
Sent: Monday, June 28, 2010 7:40 AM
To: [log in to unmask]
Subject: Re: [TN] QFP short at top of the leads

Jowan,

Was this part dipped in solder before placing?  It looks like solder has
coated the whole lead right up to the body.

Jerry

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Iven, Jowan
Sent: Monday, June 28, 2010 5:08 AM
To: [log in to unmask]
Subject: [TN] QFP short at top of the leads

Has anyone ever seen a QFP where shorts occur after soldering at the top
of the leads?
And the leads look pretty dull after soldering.  Any ideas?


A picture is available at
http://ipc-technet.groupsite.com/uploads/galleries/x/000/020/5ba/technet
01.jpg

Jowan Iven 




************************************************************************
**********************
This e-mail and any attachment is confidential and may be legally
privileged or otherwise protected from 
disclosure. If you are not the intended recipient, please notify the
sender immediately by returning this e-mail. 
Neways Electronics NV is not responsible for the improper or incomplete
transmission of any e-mail, or for any 
delay in its receipt.
************************************************************************
**********************

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2