TECHNET Archives

September 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bob Landman <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Landman <[log in to unmask]>
Date:
Wed, 8 Sep 2010 15:41:56 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (389 lines)
We use water-soluble solder flux washed with hot water-softener treated tap water on sensitive analog fiberoptics
receiver circuits.  We have never seen any leakage problems (signals as low as 1 x10-9 amps).

What concerns me is any flux residue - concerned that humidity (our fiberoptic products are used outside in climates like
Florida) so leakage from residues could cause problems.

Bob Landman
H&L Instruments, LLC

On Sep 7, 2010, at 8:22 AM, Robert Kondner wrote:

> Doug,
> 
> 
> 
>  I did forget to mention to blow the water off the board with an air gun, a
> very important step.
> 
> 
> 
> Tap water limits are about 500mg per L, at least that is my quick check on
> the web. Sounds like a lot compared to what I see here but lets use that
> number.
> 
> 
> 
> Lets assume I have a 1mm drop (1/2 sphere) per square inch of PCB, that is
> about 1/2 mm cubed. (Drops are very small after the air gun.
> 
> 
> 
> 1 L = 10**6 mm cubed. 
> 
> 
> 
> So, on my board I can expect .250g/10**6  = .25ug / in squared. Wow, sounds
> low, did I miss a few magnitudes of 10 somewhere?
> 
> 
> 
> So how bad is tap water again?
> 
> 
> 
> I saw some specs allowing 10ug/in**2 so I guess that means I can have 40
> drops of tap water per in **2. 
> 
> 
> 
> Thanks
> 
> Bob Kondner
> 
> 
> 
> 
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
> Sent: Tuesday, September 07, 2010 9:14 AM
> To: [log in to unmask]
> Subject: Re: [TN] Hand Soldering
> 
> 
> 
> Ohhhh, I beg to differ.  Water soluble fluxes are more active and will 
> 
> probably do OK for soldering, but they also represent a danger if you do 
> 
> not totally remove them or if some of it flows into places and does not 
> 
> get rinsed out.  What really makes me nervous about your approach is your 
> 
> choice of equipment and cleaners. Tap water sucks as a cleaner and hot tap 
> 
> water only slightly better.  You might be able to remove the visible 
> 
> residues, but will still have invisible residues that will cause problems. 
> 
> In some cases, you are putting on more contaminants with the tap water 
> 
> than you are removing.
> 
> 
> 
> We use low residue fluxes here on class three product and have a number of 
> 
> cases where the the residues are left in place.  It is simply a matter of 
> 
> finding a flux and cleaning combination that works well together, and 
> 
> limiting the amount of additional flux you add.  A skilled operator can do 
> 
> soldering with no more flux than is in the core of the wire. You may need 
> 
> a slightly larger core.
> 
> 
> 
> Ken, I would suggest this short list to you.  Use either Kester 245 low 
> 
> residue flux (P3 core) or Alpha Telecore Plus (also P3 core).  Both are 
> 
> standards here and work well for soldering.  For topical cleaning 
> 
> solutions, try Kyzen's Cybersolv 141b or Chemtronics Flux-Off Heavy Duty. 
> 
> Both these cleaning agents work well with the fluxes I named. 
> 
> 
> 
> Doug Pauls
> 
> Rockwell Collins
> 
> 
> 
> 
> 
> 
> 
> Robert Kondner <[log in to unmask]> 
> 
> Sent by: TechNet <[log in to unmask]>
> 
> 09/06/2010 01:27 PM
> 
> Please respond to
> 
> [log in to unmask]
> 
> 
> 
> 
> 
> To
> 
> [log in to unmask]
> 
> cc
> 
> 
> 
> Subject
> 
> Re: [TN] Hand Soldering
> 
> 
> 
> 
> 
> 
> 
> 
> 
> 
> 
> 
> 
> Ken,
> 
> 
> 
> In my mind there is absolutely no question, hand assemble using Water
> 
> Soluble flux. A good spray under hot water cleans well. 
> 
> 
> 
> During final assembly or rework I might use a no clean at spots. The only
> 
> problem is the no clean is VERY DIFFICULT to remove so don't try. It
> 
> detracts from board appearance.
> 
> 
> 
> It the spot being reworked is a sensitive analog circuit they rework 
> 
> using
> 
> Water Soluble. For anything close to fine pitch SMT you should be applying
> 
> liberal quantities of Water Soluble flux, only way to rework.
> 
> 
> 
> You can get a little "Water Pick" real cheap. Load it with hot water and
> 
> you can you can really get down into the nooks and crannies. 
> 
> 
> 
> Bob Kondner
> 
> 
> 
> -----Original Message-----
> 
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Kenneth Wood
> 
> Sent: Monday, September 06, 2010 8:30 AM
> 
> To: [log in to unmask]
> 
> Subject: [TN] Hand Soldering
> 
> 
> 
> Hi all.
> 
> What is the best setup for hand soldering as far as solder / cleaner?
> 
> Rosin core? Water soluble? No-Clean?
> 
> What cleaner too?
> 
> 
> 
> I've been using rosin core with various cleaners but I have a hard time 
> 
> with
> 
> the white residue the cleaners leave.
> 
> 
> 
> Thanks
> 
> Ken
> 
> 
> 
> 
> 
> 
> 
> 
> 
> 
> 
> ______________________________________________________________________
> 
> This email has been scanned by the MessageLabs Email Security System.
> 
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> 
> ______________________________________________________________________
> 
> 
> 
> ---------------------------------------------------
> 
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> 
> To unsubscribe, send a message to [log in to unmask] with following text in
> 
> the BODY (NOT the subject field): SIGNOFF Technet
> 
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> 
> To receive ONE mailing per day of all the posts: send e-mail to
> 
> [log in to unmask]: SET Technet Digest
> 
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> 
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> 
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 
> 847-615-7100 ext.2815
> 
> -----------------------------------------------------
> 
> 
> 
> 
> 
> ______________________________________________________________________
> 
> This email has been scanned by the MessageLabs Email Security System.
> 
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> 
> ______________________________________________________________________
> 
> 
> 
> ---------------------------------------------------
> 
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> 
> To unsubscribe, send a message to [log in to unmask] with following text in
> 
> the BODY (NOT the subject field): SIGNOFF Technet
> 
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> 
> To receive ONE mailing per day of all the posts: send e-mail to 
> 
> [log in to unmask]: SET Technet Digest
> 
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> 
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 
> 847-615-7100 ext.2815
> 
> -----------------------------------------------------
> 
> 
> 
> 
> 
> 
> 
> ______________________________________________________________________
> 
> This email has been scanned by the MessageLabs Email Security System.
> 
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> 
> ______________________________________________________________________
> 
> 
> 
> ---------------------------------------------------
> 
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> 
> To unsubscribe, send a message to [log in to unmask] with following text in
> 
> the BODY (NOT the subject field): SIGNOFF Technet
> 
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> 
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> 
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> 
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> 
> -----------------------------------------------------
> 
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2