X400-Content-Type: |
P2-1988 ( 22 ) |
Old-Return-Path: |
|
Date: |
02 Jan 97 15:59:25 -0500 |
Precedence: |
list |
Resent-From: |
|
Conversion: |
Allowed |
From [log in to unmask] Thu Jan 2 16: |
26:26 1997 |
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
Priority: |
non-urgent |
X-Loop: |
|
Content-Return: |
Allowed |
X-Mailing-List: |
|
TO: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vfvJ9-0000VhC; Thu, 2 Jan 97 16:08 CST |
Return-Path: |
<TechNet-request> |
X400-Originator: |
|
X400-Recipients: |
non-disclosure; |
Alternate-Recipient: |
Allowed |
Message-Id: |
<04B0C32CC21AD004*/c=us/admd=cwmail/prmd=carrier/o=syracuse/ou=ccmail1/s=Parr/g=Aric/@MHS> |
Resent-Message-ID: |
<"s4qcx3.0.NRB.D73po"@ipc> |
Subject: |
|
From: |
|
Disclose-Recipients: |
Prohibited |
X400-Received: |
by /c=us/admd=cwmail/; Relayed; 02 Jan 97 15:59:25 -0500
by mta MTAwltk in /c=us/admd=cwmail/; Relayed;
02 Jan 97 15:59:25 -0500 |
Content-Identifier: |
04B0C32CC21AD004 |
X400-Mts-Identifier: |
[/c=us/admd=cwmail/; 04B0C32CC21AD004-MTAwltk] |
Parts/Attachments: |
|
|
We solder both mixed SMD (bottom side and leaded) and leaded panels
with large heat sinks and 15 relays with a 2% solids no clean in air,
some panels are 6+ layers. Hole filling is not a major problem, with
the exception of specific parts with hole/lead ratios outside of our
design standards. However, I can get 100% fill with a more aggressive
flux.
The chip wave is not required on one brand of machine. I must use it
on another, most likely because of a spray fluxer issue.
______________________________ Reply Separator _________________________________
Subject: RE: ASSM: Top fillet formation
Author: [log in to unmask] at internet
Date: 12/21/96 2:41 AM
A couple of questions,
1. Are you using the turbulent wave with the lambda wave?
The added thermal transfer that the turbulent wave will add to the card may
help improve your solder filling problem.
2. What temperature is the topside of the board at before contact with the
solder wave(s)?
Going somewhat hotter then your flux manufacturers recommended temperatures
in not always a bad thing. I would think it would be better to run hotter
and get some solder up in the barrel then to run cooler and not have solder
fill. As long as components are not being damaged.
3. What type of fluxing application are you using? foam/spray
Foam may give you a little more flux up into the barrels.
----------
From: TechNet-request
To: Technet
Subject: ASSM: Top fillet formation
Date: Friday, December 20, 1996 06:34
Hello Technetters,
I need some advises. I have a 6- layers board. I try to wave solder it,
the solder
at the ground point is not able to flow up to the top side of the board, in
fact, it
doesn't flow above 75%.
We have tried using a solder-iron and set to temperature to 450 deg. cel.
and
hopefully able to force the solder through the PTH. Too bad, it didn't work
anyway
and it in fact has caused some lifted pads.
We use full blow Nitrogeneous wave-solder machine, and the flux we use is
only 1.2% solid content. And if the preheat temperature set to high, the
flux
gets degraded before it even reaches the wave..
I would like to know if anyone could advise me how wave-solder such a board
with a great heavy thermal mass.
Thanks in Advance..
=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-==-=-=-=-=-=-=-=-=-=-==-=-=-=-=.
/ Kong Hui Poh /
/ Techgate /
/ - The Technological Gateway - /
/ Email Add: [log in to unmask] /
/ /
/ Fax Number: (65) 842 0318 /
/
............................................................................
................................../
/_________________________________________________________________/
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|