TECHNET Archives

April 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Tue, 30 Apr 2013 10:25:19 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (104 lines)
Yeah Rex, you're right. I remember being told one time that sometimes
x-ray allows you to see TOO much and causes you to worry about things
that you shouldn't...  :o) 

Steve 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rex Waygood
Sent: Tuesday, April 30, 2013 10:14 AM
To: [log in to unmask]
Subject: Re: [TN] Pic of head-in-pillow for the site

And probably has no detrimental effect on reliability.
Rex

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski
Sent: 30 April 2013 17:05
To: [log in to unmask]
Subject: Re: [TN] Pic of head-in-pillow for the site

Thanks, Steve.

That void measures < 25%. Not optimum, but conforms to IPC-610 Class 2.

Ed Popielarski
Engineering Manager

[Description: FullLogo]
                               970 NE 21st Ct.
                              Oak Harbor, Wa. 98277

                              Ph: 360-675-1322
                              Fx: 206-624-0965
                              Cl: 949-581-6601

https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn
=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A

From: Steve Gregory [mailto:[log in to unmask]]
Sent: Tuesday, April 30, 2013 8:55 AM
To: Ed Popielarski
Cc: [log in to unmask]
Subject: RE: Pic of head-in-pillow for the site

Hi Ed!

Nice image! Got it posted, it's here:

http://stevezeva.homestead.com/Head-in-pillow_X-Ray.JPG

What about the void off to the right? Is there any concern about that?

Steve Gregory
Process Engineer
Kimco Design and Manufacturing
652 N. Five Mile Road
Boise, ID 83713
(208) 322-0500 Ext. 3133

From: Ed Popielarski [mailto:[log in to unmask]]
Sent: Tuesday, April 30, 2013 8:58 AM
To: Steve Gregory
Subject: Pic of head-in-pillow for the site

Hi Steve,

I have a good X-Ray picture of a head-in-pillow that Leland would find
helpful. If you don't mind posting it for him?

Ed Popielarski
Engineering Manager

[Description: FullLogo]
                               970 NE 21st Ct.
                              Oak Harbor, Wa. 98277

                              Ph: 360-675-1322
                              Fx: 206-624-0965
                              Cl: 949-581-6601

https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn
=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2