FeinFocus is now merged with Yxlon.
 
 
 
In a message dated 8/26/2009 6:42:33 A.M. Eastern Daylight Time,  
[log in to unmask] writes:

Kevin,

Since it has not already been mentioned, you could also  try Phoenix X-Ray -
http://www.phoenix-xray.com/en/products/ as an  alternative to Dage

Is Fein Focus still in business??

MIS  Testing Services - in Canada  http://www.miselectronics.com/index.php


My assumption is that the  device is either not conducive to acoustic
microscopy, or you don't want to  get the boards wet.  Sonix
http://www.sonix.com/products/index.php3  
and/or Sonoscan http://www.sonoscan.com/ 

May your joints be free  of voids!

Steve C



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2