We use Humiseal 1A33 coating. Whe have used Humiseal 1063 stripper but without much accomplished. Will take 8- 10 hours before anything happens. This is just unacceptable. Other products have left residue under BGA's or have been corrosive enough to pit solder joints or remove component markings. Some semipastes or gel like products have left residue under leads and so on and so on. So you see that is why I have asked the question. Actually, bead blasting was a mechanically technique that sound promising. Removed the coating quite fast but left blasting media under some components that I could not wash out.
Andrew Kettlewell
-----Original Message-----
From: Edward Mines <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, 14 Dec 2005 07:22:02 -0800 (PST)
Subject: senior chemist at HumiSeal
I was the senior chemist at HumiSeal for 12 years.
Different polyurethane conformal coatings require different strippers. Do you know which one you was used? Is it yellow?
Be careful which stripper you use. Some of them can attack components.
Edward Mines BEChE, MEChE
238 Willard Dr.
Hewlett, NY 11557
516 205-6523
Yahoo! Shopping
Find Great Deals on Holiday Gifts at Yahoo! Shopping
___________________________________________________
Try the New Netscape Mail Today!
Virtually Spam-Free | More Storage | Import Your Contact List
http://mail.netscape.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------